Product

Stellite alloy 6 Strips For Steam Turbine Blades

The last stage blades of the steam turbine are prone to water corrosion, and the failure of the blades leads to the unsafe operation of the steam turbine. The stellite alloy blade anti-corrosion sheet properly solves the problem, and the stellite alloy anti-corrosion sheet is welded to the blades by brazing. , effectively prevent the water corrosion of the steam turbine blades, and improve the safety and economy of the normal operation of the steam turbine.

  • SYTOP
  • China
  • 20-35days
  • 3000pcs/ month
  • Information

Stellite alloy 6 Strips For Steam Turbine Blades

Stellite alloy 6 Strips

Stellite alloy strips are welded to steam turbine blades. Stellite alloys have high hardness and good toughness, small variation when water droplets hit, good resistance to water corrosion and erosion, and high microstructure stability, although beyond a certain range Water corrosion will also occur, but the ability to resist fracture is good, and even if serious water corrosion occurs, it is not easy to produce cracks. At the same time, different shapes of alloys can be selected according to the operating conditions. When the water corrosion is serious, a new Stellite alloy sheet can be replaced, which is very suitable for the working conditions of the blade. Therefore, when welding Stellite alloy, the most commonly used method to prevent water corrosion of steam turbine blades method.


1.      Stellite  alloys have higher melting points than nickel (or iron) alloys ,This gives them the ability to absorb stress to a higher absolute temperature .

2.      Stellite  alloys give superior hot corrosion resistance to gas turbine atmospheres , this is due to their high chromium content.

3.      Stellite  alloys show superior thermal fatigue resistance and weldability over nickel alloys .

 

---Excellent wear and corrosion resistance even at high temperature up to 800


Chemical compositions and properties (%)

Brand

C

Mn

Si

Cr

Ni

Mo

W

Co

Fe

P

S

Density

(g/cm3)

Hardness

(HRC)

stellite 3

2.0-2.7

1.0

1.0

29-33

3.0


11-14

Bal.

3.0

≤0.03

≤0.03

8.55

51-55

stellite 6

0.9-1.4

1.0

1.5

27-31

3.0

1.5

3.5-5.5

Bal.

3.0

≤0.03

≤0.03

8.35

38-44

stellite 12

1.1-1.7

1.0

1.0

28-32

3.0


7.0-9.5

Bal.

3.0

≤0.03

≤0.03

8.40

44-49

stellite 20

2.2-3.0


2.0

30-34

3.0

1.0

14-18

Bal.

3.0

≤0.05

≤0.05

8.65

53-59

Tantung-G 25

2.2-2.8

1-3


27-32

7

Ta/Nb

14-19

Bal.

2-5



8.84

57-60

Tantung-G35

3.3-3.8

1-3


27-32

7

Ta/Nb

14-19

Bal.

2-5



8.80

60-63

Tribaloy 400

0.04


2.5-2.7

8-10


27-29


Bal.





55

Tribaloy 800

0.04


3.2-3.6

16-18


27-29


Bal.





58

 

SYTOP cobalt base alloys is a range of cobalt-chromium-tungsten alloys with wear resistance, corrosion and high thermal resistance. It is widely used in oil & gas, machinery, wood cutting, automotive, paper and food processing industry etc.

 Stellite alloy Strips


Specifications that we can made :

 

Different size bars , rods , ingots , plate 

Drawing made seal , valve seat and ball , bush and sleeve etc. 

Some size tube

 

Most of our products are made upon request so contact us right now for personal and professoinal service. 


More details about cobalt chrome round bar please do not hesitate to contact me . 

Get the latest price? We'll respond as soon as possible(within 12 hours)
This field is required
This field is required
Required and valid email address
This field is required
This field is required
For a better browsing experience, we recommend that you use Chrome, Firefox, Safari and Edge browsers.